Rod: Al-(3-6%)Ti-(0.1-0.5%) C
Chemical Composition: Ti 3-6% C 0.1-0.5% Fe ≤0.20% Si≤0.20% Al remaining
Application and Characteristics: aluminum alloy agent used for aluminum and its alloys'' grain refining to improve its perforance. Simples to use, little application amount but great effect. Widely used in aluminum casting industry.
Package: 100g per piece, 200g per piece, 350g piece or 500g per piece
instructions on application:
1. Roast to dry before use
2. Adding temperature: 680oC-780o
3. Application amount: determined by actual experiments and dosing calculation
4. Adding method: rake open the floating scum, drop the rod into molten aluminum, and
stic the metal up to evenness.